The easy open end on the defective sterilization

EOE those defects affect the sterilization of it? Here the production of a variety of beverages covered by professional, Lid and Aluminum EOE - packaging plant in Dongguan real promise to you briefly explain it, I hope for your help.

1, seaming poor - in cooling the cooling water tank into the bacteria, resulting in deterioration of the beverage.

2, sealants poor quality - not fully fill the gap seaming, cooling water will cause the bacteria into the tank again, leading beverage spoilage.

3, the outer coating bad - can not withstand high temperature and pressure, coating cracking or blistering, black rivet parts most likely to rupture.

4, tangent too - when the cooling tank pressure is higher than the tank, easy to burst from the tangent position.

 